    PMC Standard and Gold both shrink 30% since they are fired at the
    maximum times and temperatures for each medium. 

    PMC+ and 3 shrink 10-12% depending on the schedule you choose.  When
    fired at 1650 for two hours they reach maximum shrinkage of 12%, if
    you have rehydrated and added water to the clay, it may shrink a tiny
    bit more, but no where near 30% 

    The times and temps suggested by the manufacturer of Precious Metal
    Clay are as follows: 

    PMC Gold - 1830 for two hours
    PMC Standard - 1650 for two hours
    PMC+ - 1650 for 10 mins OR
                  1560 for 20 mins OR
                  1470 for 30 mins
    PMC3 - 1290 for 10 mins OR
                  1200 for 20 mins OR
                  1110 for 30 mins

    Art Clay Silver shrinks 8-10% and has a different firing schedule. 
    They never developed a material that shrinks 30%. 

HTH,
Lora Hart

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project