>       Is there a fairly accurate method to guestimate how much a model
>     made from green wax might weight in silver?  The wax model weights
>     about 2.5 grams.. 

    If you have a scale: multiply the weight of the wax by the specific
    gravity (density) of the desired metal, in this case 10.5. 

    If you don't have a scale you can use the water displacement method.
    Put water in a tall skinny cylinder. Mark the top of the water level
    on the glass with a sharpie or china marker. Submerge the wax under
    the water, and mark the new, higher level on the cylinder. Remove
    the wax, make sure the water level is up to the first mark on the
    cylinder. Add metal until the water reaches the upper mark.
    Warning!! If you use this method for calculating your weight, make
    sure you dry the metal thoroughly or your casting will be porous. 
    Don't forget to add some metal for the sprue. Tyler Teague wrote some
    excellent articles for AJM Magazine on proper sprue angle and
    buttons. 

Have a great day!
Kate Wolf in Portland Maine
http://www.wolfwax.com
http://www.wolftools.biz
http://www.katewolfdesigns.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project