Hi James,

>     Most of the colored drusy is dyed. 

    A bit of an overstatement, I think.  If you're talking about
    quartz/agate drusies, then maybe.  But others are usually *not* dyed:
    uvarovite, melanite, malachite, azurite, psilomelane, cobalto calcite
    (or dolomite, if you prefer), smithsonite, pyrite, cornetite,
    kammererite and more.  And even where the quartz/agate drusies are
    concerned, there are plenty of natural stones in blues/greens
    (chrysocolla & blue chalcedony or lace agate), yellows/tans/oranges
    (Brazilian agate and  petrified coral), browns/beiges (petrified
    woods), purples (amethyst), and more. 

    Chances are, what Dave has is dyed, but I wouldn't be positive
    without seeing it. 

Beth

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project