>        when you braze steel, how hot are you getting, do you have to
>     apply any flux to the metal pieces you are joining? 

    BJ, you can buy brazing rods coated with flux, but I can't recommend
    it because the coating tends to crack and fall off.  In my opinion,
    it would be better to do one of two things.  Either buy the black
    flux which is available at welding shops and is stable at higher
    temperatures than the usual flux for silver soldering, or buy a can
    of dry flux meant for brazing and dip your brazing rod into it
    periodically as you are brazing. 

    As to how hot you need to get, in order to braze,  check the melting
    point of the brazing rod.  The metal you are brazing must get at
    least that hot, in the area of the braze.  If you are brazing large
    pieces of metal, you will need an oxy-acetylene torch, in order to
    get and keep the metal hot enough for the brazing rod to flow.  

Hope this helps-- 
Judy Bjorkman

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project