>     ... even the round noses mark the sterling slightly when I join the
>     jump rings in preparation for soldering. 

Hello Cathryn,

    Here's a few suggestions: 

    - don't use the round nose pliers, use flat nosed ones instead
    because they spread the pressure out over a larger area and are less
    likely to dent the metal. I knocked the sharp corners off of a spare
    pair I had so they're much less likely to nick the metal. 

    - use parallel jaw pliers.  They grip better with less pressure. 

    - make little booties for your pliers from copper sheet (I'm using 36
    gauge sheet. Easy to work with but booties made from it will wear out
    after a while). 

    - teach yourself to use only the necessary amount of pressure to get
    the job done and no more.  This goes a long way to reducing plier
    "tracks". 

    In my experience the bottom line is that the best way to deal with
    plier marks is to not put them there in the first place. 

Cheers, 
Trevor F. 
in The City of Light

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project