>     I read somewhere that silver returns more reflected light than any
>     metal. is it true? 

Hello X,

    Yes, it is true.  Mark Grimwade's "Introduction to Precious Metals"
    (if you can get a copy , DO IT, great little book!) plots the
    reflectivity of the various precious metals in terms of wavelength vs
    reflectivity (in other words different colors vs amount reflected). 

    Silver outpaces all the others straight across the board.  It varies
    from around 80% at the shorter wavelengths to just under 100% at the
    long end. 

    Gold starts really low, under 50% at the low end, but increases
    rapidly --more so than any of the others-- to just under silver's
    marks, say 95%, at the long end. 

    Rhodium varies from 70% for the short to about 80% at the long end. 

    Platinum goes from 45% at the short end to about 70% at the long end. 

    Highly polished silver looks super bright and white-ish for a good
    reason. 

<edit>

    Introduction to Precious Metals
    By Mark Grimwade

    http://www.ganoksin.com/jewelry-books/us/product/0408014512.htm
    Price: $15.95

    Media: Paperback
    Manufacturer : Newnes
    Release data : March, 1985

</edit>

Cheers, 
Trevor F. 
in The City of Light

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project