From: Cathryn Date: Sat Apr 02 19:26:58 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I've started building chains out of fat sterling wire - 2mm wide. After tumbling, they look truly handsome. However, eagle eye here is bothered by the tiny marks left by my pliers - even the round noses mark the sterling slightly when I join the jump rings in preparation for soldering. Who on Orchid has solved this problem? I've tried wrapping the pliers with different kinds of sticky tape, but it inevitably slips, making the join not solder perfect. Helpful hints really welcome Thanks Cathryn ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project