From: Elaine Luther Date: Thu Mar 17 20:08:01 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== You can use PMC with polymer clay. Here's how it is most commonly done: Make your piece in PMC, usually creating an opening or bezel of some sort with the PMC. Fire and polish. Make a polymer clay whatever, to go into the space created in the PMC. Bake the polymer clay in the oven at 275 for 20 minutes. You can't do it the other way around, can't put polymer clay in the kiln. Elaine Elaine Luther Metalsmith, Certified PMC Instructor http://www.CreativeTextureTools.com (TM) Hard to Find Tools for Metal Clay ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project