>        I'm curious to know if you plan to eventually re-cut this
>     sapphire yourself? I'm not at all a world-class faceter, and would
>     be nervous about it, myself. 

James,

    No need to be nervous about recutting such a stone.  If the original
    cutter did any thing right at all, they probably did a proper
    orientation for their original cut.  That makes the stone a perfect
    preform for recutting.  Often when recutting such a stone, the loss
    is actually quite minimal.  I have a .56 ct natural ruby (absolutely
    beautiful stone) what had been badly cut by the native cutter.  It
    was an oval and they had left a very bad fractured area in the culet
    which also had a black inclusion in it.  I recut the crown using the
    original design but tightening up the facets and improving the
    polish, then redid the pavillion in a slightly different design
    cutting the fracture and inclusion away.  In the end it came to
    exactly .50 cts and tripled in value! 

    It would be an excellent project for a faceter wanting to expand
    their horizons!  In this case, a couple more degrees on the
    pavillion mains would probably do the trick.  The stone would become
    slightly deeper and loose a bit of girth but the results would be
    worth it. 

    Cheers from Don at The Charles Belle Studio in SOFL where simple
    elegance IS fine jewelry! dcdietz AT comcast.net

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project