>       To my knowledge there is nothing that can be done in PMC that
>     cannot easily be done with either metalsmithing or casting
>     techniques. 

    Perhaps, but these things can be done *faster* in PMC than through
    traditional methods. 

    I find all of this exhausting.  On the metal clay list, there's
    constant yacking about which is better, PMC or Art Clay Silver,
    which I find dull.  On Orchid, whenever the subject of PMC comes up,
    people decry and say how horrid it is. 

    It's just a tool. 

    No one ever decrys wax and says wax should never be used! 

    I don't understand why metal clay generates such strong feelings. 

    If you don't like it, if you don't need it, don't use it. 

    Many people like it and many people don't want to learn
    metalsmithing. 

    For many of my students, learning to work with metal clay has
    enriched their lives.  PMC in particular, and metal clay in general,
    are here to stay.  They have a place. 

    Just try not to hate it so much, eh? 

Elaine
Elaine Luther
Metalsmith, Certified PMC Instructor
http://www.CreativeTextureTools.com (TM)
Hard to Find Tools for Metal Clay

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project