From: Katherine Palochak Date: Thu Mar 10 19:41:32 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== The best way to get rid of these stains is with a simple pickle that someone put out there a long time ago. Some wizard (Peter Rowe? Tim McCreight?) developed a recipe for peroxide pickle that works wonders. Formula: 3/4 C. drugstore strength hydrogen peroxide, 1/4 C. grocery store strength white vinegar. Get it hot but not boiling. Pickle with this, makes it all pink; then put it in the Sparex pickle, pink gone. Repeat as necessary. Good for light firescale too. If you're coming up with the stains immediately after etching, before soldering, this means you need to neutralize the metal better after etching. Use clear household ammonia in a 1:8 ratio with water. Let the piece set for 15 minutes and scrub well with a toothbrush. Rinse in water. Should solve your problems. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project