Beverly,

    I'm not sure what you mean by 'sponge coral'.  The only thing I can
    think of is dead coral that has partially deteriorated or been worm
    eaten.  Back in the days when Taiwan was a world leader in
    carving/cutting coral for the world market, I used to see quite a
    bit of it being brought in by the dredging boats.  A good friend who
    owned a coral cutting/carving factory, explained what it was and how
    it was worthless.  Essentially, it was just coral with lots of holes
    in it!  Right...it looked a lot like a sponge.  It still showed the
    original color of the coral; red, orange, pink or whatever, but
    otherwise, it was ugly. 

    If what you are talking about is the same stuff, it doesn't have any
    effect on the environment because its already dead, except maybe
    removing some materal that other coaral might use in reef building. 
    On the other hand, if they are dredging it, they proably are doing
    human damage to the reefs. 

    Cheers from Don at The Charles Belle Studio in SOFL where simple
    elegance IS fine jewelry! dcdietz AT comcast.net

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project