| [Orchid] Working with 14/20 Gold filled stock | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: Larry Date: Tue Mar 08 16:24:54 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I have worked in sterling silver and karate gold and have done OK but my first piece using gold filled stock did not turn out. Are there specialized instructions for soldering gold filled stock that I should be aware of? The solder did not act as I thought it should or at least not like when I am working silver. I use the alcohol/borax flux. I do have other flux for gold I could use. It seemed like I had to get the whole piece a lot hotter before the solder would flow. I believe this then caused the surface gold to melt and mix with the base metal so that the appearance was very splotchy. It came out a coppery color (unless this was from putting it in the pickle). Is there any written material about working gold filled stock? Also what techniques or guidelines should be used in finishing/polishing a piece since the gold is just an outer covering. Larry E. Whittington New web address. http://www.geocities.com/ishoulddof2003 ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project