    For my copper cleaning---including large etched pieces  which are to
    be enameled,  I use a simple home recipe which works just fine.  1
    cup of salt, 1 cup of vinegar, 1/4 cup of flour.  Mix well and
    apply. It works just fine After cleaning with it, I neutralize any
    acid residue with a mix of ammonia, liquid detergent, and some simple
    green. I just sort of mix this last batch  together without measuring
    and use it as it not only neutralizes but  removes any grease. It is 
    my all purpose cleaner.  Sometimes I even toss in a little 409.
    Nothing has exploded to date, so I am sure it is a perfectly safe
    concoction. 

    Also, for  those interested in getting a green patina on  copper,
    just smear on a light coat of  the salt, vinegar, flour mix. Let it
    rest a while, rinse off,  and  you  will have a great patina. As my
    purpose in using the cleaner is not to get a patina, I have not given
    it the test of time so don t know how permanent it is. Just giving
    you this exta tidbit in case you want to try it. 

    I have heard  that Penny Brite Copper  cleaner is excellent, but as
    my home brew works so well I have not bothered to change over to
    using Penny Brite 

Alma


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project