    I'm trying to make mitsuro wax. I made the first batch this week
    Following the directions that i gleaned from a number of different
    writers on Orchid. 

    I melted the bees wax at 300F, using a temperature controlled
    Skillet, and then slowly added powdered pine resin, stirring to help
    it Dissolve. I found the the resin would get pasty and fall to the
    bottom of The pan in which I was melting it. The resin formed "globs"
    on the bottom Of the pan. To assist in dissolving the resin, I
    gradually increased the Temperature of the skillet to about 450F.
    More of the resin seemed to Dissolve. At this point I added
    microcrystalline wax to the mixture and Thoroughly mixed it in. 

    I cast the molten wax through cheese cloth into a silverstone cookie
    Pan and let it cool. The cheese cloth captured a significant amount
    of Undissolved pine resin. The wax sheet looked fine. The sheet was
    easily Removed from the silverstone cookie an by just twisting the
    pan slightly. 

    the formulation that I used was: 

    bees wax-------------------- 400 grams
    pine resin ------------------- 100 grams
    microcrystalline wax---------- 50  grams

    I've tried to "work" the wax by stretching it to develop the
    Texture, but it stretches very little before breaking. 

    can anyone who has made mitsuro wax offer any advice on how to get a
    Better result?? 

you assistance is appreciated.


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project