========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Rhona - there are several keys to drilling without cracking the glass:- 1. keep the glass cool by keeping it under water; 2. use a diamond drill bit (other types will barely scratch the surface); 3. drill slowly - I use the traditional bow drill, although one can use an electric one; 4. make sure the back of the glass is supported (for example on a small block of wood) so when the hole is drilled through it doesn't chip on the reverse. Even better, drill half way then reverse & meet it the other way. Hope that all makes sense. Works on enamels too! best, Deborah Miller ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project