>     Thanks to James for this tip, but how do you achieve that 50/50
>     ratio of a liquid and a solid?

    Perhaps I stated it incorrectly. I start with a clean, empty Skippy
    Peanut Butter jar. First, I fill it approximately one quarter full
    (by volume) of boric acid. Then I fill it to half (again, by volume)
    with denatured alcohol. Finally, I shake until it is as dissolved as
    much as it will get. In my world, that's 50/50. And no, the boric
    acid doesn't completely dissolve into solution and I never claimed
    it did. 

    This is the ratio I use so that I can replenish evaporated alcohol
    as needed. The classic recipe for this firecoat (or flux, if you
    prefer to call it that) is to add boric acid to alcohol until
    saturated, and agitate before use. You may fill the jar three
    quarters full of boric acid if you 

    wish, with the remaining one fourth alcohol, and agitate before use.
    It doesn't matter, you'll still have the same saturation of solution
    when you use it. It isn't a critical recipe. 

James in SoFl

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project