>         So I'm going to have to draw it, which is no big deal except I
>     can't remember how to draw half-round from round other than by
>     soldering together two pieces of round wire and drawing it that
>     way.  Which I don't want to do because of the issues of solder
>     tarnish.  It would be a shame to have my lovely virtually
>     untarnishable Argentium work of art (yeah right!) streaked with
>     solder tarnish at odd spots along the length of the wire.... 

    You only need to solder the first half inch, or so, of the wires
    together. Enough to form the taper that is held in the pliers.
    Chances are that the two wires will twist as they go through the
    draw plate, so it is a good idea to use a vane made from thin metal
    to guide the wires into the plate. 

>         So can anyone tell me how to draw half-round wire from a
>     single piece of round wire?  Like what size to start with in the
>     round wire to get the desired size in the half round... Ditto for
>     square wire from round wire, for that matter. 

    'cors you could just buy half round or square draw
    plates................ 

Bill Bedford

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project