    Any time you are using a steel or brass brush on another metal
    surface you need to use a soapy water lubricant, and enough of it. I
    usually rig up a drip onto a rotating brass brush, or if doing it by
    hand will dip it. If you do not use a lubricant then metal can be
    transferred from the brush to your surface. This can be done of
    purpose, as when blacksmiths brass brush steel hot without a
    lubricant, the brass transfers to the high spots on the steel with is
    black and thus everything gets greater contrast and looks
    interesting, the tops golden and the recesses black. 

best
Charles

Charles Lewton-Brain/Brain Press
President, Canadian Crafts Federation
Box 1624, Ste M, Calgary, Alberta, T2P 2L7, Canada
http://www.brainpress.com/, 
Tel: 403-263-3955  Fax: 403-283-9053  
brainnet AT telus.net

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project