From: Roger Dery Date: Sat Feb 12 00:33:09 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Noel, > I have read about the use of solutions that match the RI of > stone to reveal the internal condition of the rough. What I want to > know is, are there things I can use that I would have around, or do > I need to buy special substances for this purpose? There is a substance used by cutters called: "Refractol". It is odorless, non-toxic and has a Refractive Index of 1.567 - which is very close to Beryl - such as the Aqua you are working with. Using Refractol, you should be able to clearly view into most gem rough that has a low-to-mid RI range. In addition, you may find it helpful to use a low-intensity light, back lit of the rough you are viewing. When I need to use Refractol, I generally wear the same pair of latex style gloves. This helps to keep my hands clean and to not transfer substances from one item to another. Then, you will need to clean the rough thoroughly with denatured alcohol or your favorite de-greaser/cleanser prior to dopping. Roger Dery gemdigital AT hotmail.com Spectral Gems, Inc. Rare Gemstones - Exceptional Faceting - Genuine Colored Stones ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project