From: Michael Honeycutt Date: Thu Feb 03 10:12:14 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I have had some success with a type of solder called Fos-Flo #7. I bought it at IJS in Albuquerque. It's advertised in their catalog as producing a light copper colored seam when used correctly. In my experience it's a pretty good solder but you have to be very careful not to overheat the stuff. If you overheat it it tends to, well, I call it "flash". You still get a fairly decent join but it leaves a silver colored stain that's a bear to get out. However, IF you control your heat carefully, it won't "flash" on you and it does produce what I think is a light copper colored seam as advertised. It just takes a little practice with the torch, solder and some copper to get it right. Here's a bit of data on it: Melting temp: 1310*F or 710*C Flow temp: 1350*F or 730*C Composition: 92.75% copper, 7.25% phosphorus I use good old handy-flux with good success. Hope this helps or at least provides another option for your consideration. I don't work for IJS or anyone else for that matter. This stuff just works for me. Mike ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project