Sojourner:

    I have the same problem with my Oxy Acetylene Smith Little Torch, I
    believe it has something to do with the temperature of the tip,
    causing a faster oxidization of the Acetylene during combustion, this
    is especially more noticeable with the smaller tips, I've learned to
    manipulate the valves and either increase the fuel or decrease the
    oxy with my thumb, and not pulling the torch off the work piece to
    adjust it, that92s the nice part of having the valves at the top of
    the torch. If we are having the same problem you will notice that it
    happens a minute or two after igniting the flame, Regarding your gold
    to silver problem I solder 10k gold to silver quite often with no
    problems, also higher karat as well, just use easy or medium silver
    solder or use a 10kt easy flow solder either way works, I like the 10
    k easy flow if the joint is going to be in a place prominence and
    easy to see, other wise use silver solder. 

    Now chant the mantra  " spring is coming,  spring is coming" 

Kenneth Ferrell


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project