From: kevdan Date: Sat Jan 29 11:47:54 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I use a dental kiln it is bttom loading you put the stuff on a tray and it raises up into the kiln I have used my neycraft kiln as well but this dental gismo is awsome mine is manual but I have afriend who is a dentist and his is fully programable to rise slowly to preheat the piece and remove all moisture so you dont get pits and stuff. I got mine at a demolition yard ( I have no idea why it was there) I paid five bucks for it my friend bought his new and paid 4000 but I have seen them on ebay for a couple hunderd mine is made by jelrus. bottom loading is great you dont burn your hands and no heat escapes it maintains a perfect temperature all the time plus kiln furniture is so easy to position when your hands arent on fire. Kevin ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project