========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Peter !! I have tried your suggested combo of vinegar, salt and coffee bag, and it works!! "Really well" thank you soooooooo much, you have made life so much easier for me. I didn't just add the odd bead and piece of silver, I added whole necklaces of intricate beading, and Pazzzz am!! they where tarnish free. Usually I have to replace findings when they tarnish, its just impossible to polish thousands of head and eye pins when they are in the mix of a beading tapestry of sorts. So "thank you " thank you" and once again "thank you" Yours very sincerely Tina Ashmore Dublin, Ireland ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project