From: Daniel Grandi Date: Thu Jan 27 19:03:23 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I Agree with Peter Row that the metal Blob problem is not caused by Standard (copper/silver) sterling alloy. I'm 99% sure of is that it is caused by Some form of DeOx sterling... There are many deox sterling alloys on the market and having tested about 8 varieties, I can remember seeing some black blobs on castings ... It was caused by overheating the metal and /or using a high oxygen concentration in the flame. It is definitely possible to bring out some black ooze on certain deox materials when it is heated too far.. Some of these alloys contain metals like Tin and other low melt materials that can come out of the alloy when over heated. Hope this is helpful. Daniel Grandi Racecar Jewelry Co. Inc Tel: 401-461-7803 ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project