Hi Jessee

    I was the one who mentioned it was messy and it's both a lot of
    shavings and chewy.  But, I just took out a piece (It's at least 23
    years old.) and tried to file it to be sure and it's not quite as bad
    as I remembered. The edges get chewier than the flat places. I
    couldn't find my large rods but the small rod I found had yellowed a
    bit but was creamy white under the slight surface film (probably
    oil).  

    I got my end cuts at a plastic supplier that dealt mostly in plexi. 
    It might have been Cadillac Plastics. The white was in rod form, the
    black was in a small block.  I found several suppliers on the web so
    you might be able to find one that would sell you a small quantity. I
    just checked the Small Parts site
    (http://www.smallparts.com/materials/) and they list both black and
    natural(white)sheet and rod. 

Linda M 
lmog AT midtel.net 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project