    recently had a similar problem using cerium oxide grit and silver.
    You'll need to 

    1: Clean the tumbler.
    2: Clean the piece (I ultrasoniced mine)
    3: Clean the shot
    4: use a descaling solution and stainless steel shot in the final     
    tumble.

    Oh you also might have some wax in your tumbler due to the rouge
    compound.... In which case I would suggest running some stainless
    shot in it for 24 hours with rubbing alcohol instead of tumbling
    solution, that will clean off the shot and get the wax out of any
    perforations in the rubber of the tumbler barrel. 

    That's what worked for me... If you are still having problems after
    doing that particularly if the silver is still pewter in color.
    Repeat the above process but before step 4, run the piece thru with
    some fine plastic abrasive. 

    PS - what type of solution are you tumbling in and what is the total
    time for your tumble cycle? 

Hope that helps,
Jon P

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project