========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I am sorry to disagree with Mr. Rowe but I feel that it is very unlikely there is any "microalloying" going on between titanium and gold...This would only happen at expremely elevated temeratures and the process would take time...It would be happening through the process of dissolution which requires time and residence "or contact:" as liquids....I don't see it as possible. I am very doubtful about it...( I have been in the ti industry 15 years and can tell you from experience in the manufacture of titanium alloys)... You could be getting dust contamination if your surroundings are not kept clean but the dust will be highly oxidized ( and pacified) and unrecognizable as titanium as an element. It does have different coefficient of xpansion tendencies from gold so you could be getting stresses as opposed to contamination. I am interested in what you are seeing...Tell me more Scott Jackson Tinomics Inc. #1 Tom Rab Lane SW Ft Myers, Florida 33907 330-412-1767 cell 239-425-0715 office 239-425-0716 fax scoot77 AT aol.com Tinomics makes small titanium castings for jewelry, medical, consumer and aerospace markets. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project