Hi Connie,

    If the yellowing occurs only where you are working...ie the sizing
    spot... then the solder or the stock you use to size the ring might
    be the culprit. 

    My best guess though is you are experiencing the problem associated
    with rhodium plated merchandise from the factory.  After sizing you
    obviously need to polish, which removes the rhodium finish in that
    area. You'll need to polish and re-rhoduim the whole piece for the
    same bright white look. 

    A rhodium set up is not complicated but can initially cost some $ to
    the store. You'll need a rectifier, beaker, plating anode, and
    rhodium.  The rhodium is the most expensive component but should last
    a long time as long as you don't contaminate it. 

    Check out stuller and ask them about your options and safety issues.
    You don't need a large rectifier for doing repairs. 

    With chains you will have a more difficult time getting the plating
    to come out well. A good fire coat on the chain and restricting the
    area of heat as best as possible will help so you can do a touch up
    polish of just that area. 

Good luck,
Mark

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project