    Don, I'm sorry to not have an answer for your problems but it seems
    to me that you are dealing with a super-saturated solution. I mean
    that, at boiling temps, the water is able to hold more of your
    chemicals in a disolved state. After it cools down to room temp it
    has lost some of its "holding" capacity and a certain amount of the
    chemicals precipitate out of the liquid. That would explain why the
    clear liquid works well at room temps. It is still a super-saturated
    solution but just at a lower temp. I've had similar issues with
    home-brewed pH Minus pickle. Hot it's a clear liquid, cool it down
    to near freezing and it forms a crystaline matrix at the bottom of
    the pot. Heat it up again and the crystals go away. 

    A question I have is where to get the TSP? I've called several
    places and gotten lots of runaround. I'm sure I'm missing something.
    Hope this helps some. 

Mike

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project