From: samuel olin Date: Fri Jan 21 22:04:33 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== quaro Try using 4pieces of the local news paper folded in half and in half again til it is 1 or 2 inches larger then your flask. Cut a hole in the center half the diameter as your flask let it soak in water till saturated 2 to 3 min pless out extra water .Now you have a gasket that will not leak. Yes you will get a bit of water in your pump but this is removable as oil floats on water . also even if you have to change out your oil more often it is better then loosing a flask to no vacuum I do alot of casting and my fellow jewellers who do in shop casting use this method .it works well any questions please email them to me samolin AT hotmail.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project