========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Bart, The pinkish color you refer to is most likely the copper alloy. It is best to use a coating on the work such as Alcohol and boric acid to protect from firescale. It is also important to stop and Pickle the piece often if you are doing a lot of work on it. The lower the karat of the gold the more obvious this problem becomes if you are heating the piece multiple times without Pickling and cleaning the piece. Pickle will only remove the surface oxidation. If you have overheated the metal and the oxidation goes deep into the metal you will have to take drastic measures to remove it such as Stripping or Bombing and even then it may not remove the oxidation if it is extremely deep. Good Luck Greg DeMark email: greg AT demarkjewelry.com Website: www.demarkjewelry.com Custom Jewelry - Handmade Jewelry - Antique Jewelry ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project