    Thank you everyone who responded to my deep-draw question!  Your
    collective wisdom is 'deeply' appreciated. 

    I had a very exasperating problem with my last batch of castings,
    and I am at a loss as to what's going on. 

    I have a table-top vacuum machine, the kind that uses a solid flask.
    Lately, I have not been able to get a seal on my flasks.  Thanks to
    the Ganoksin tips, my spruing has improved to the point where
    bubbling is minimal even without a seal, but it is still a problem in
    some cases. Since I'm under a deadline to get out a bunch of pieces,
    I can't afford to have a significant failure rate.

    Changing pads hasn't helped.  The machine is pulling a vacuum (I've
    tested it every time), but I just can't get the flasks to seal.  I'm
    thinking of gluing the pad down in case air is seeping underneath.
    Pushing down with the tongs has no effect.  The investments don't
    appear to have any cracks, and there aren't any blow-outs through the
    bottom.

    I would be grateful for any tips or suggestions. 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project