Hi Bethany

    I've machined Delrin on a metal lathe to use for stoppers for a
    woman's dresser set of sterling perfume bottles and a cream jar. The
    Delrin created a tight seal for the bottles. I've also carved it and
    used it as part of a silver brooch. It carves very nicely with
    simple woodcarving tools and can be shaped with files and emery
    papers (filing is a bit messy) but does take some effort. It machines
    beautifully.  My favorite finish for it was to emery it to 600 while
    it was still on the lathe and then to cut it off and pumice it. For
    the brooch I took the carving to a high polish. It was a long time
    ago. I don't remember doing anything special so I must have polished
    it with White Diamond and then perhaps rouge but the Delrin I
    polished was black so I'm not sure how those compounds would work on
    white Delrin. I think White diamond on a new clean buff would work. 

HTH 
Linda Moughemer


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project