    I have always used  Prips flux to prevent firescale on my silver.  I
    have bought the Prips commercially and also used that made by others
    in our shop. 

    Recently I have tried mixing up some myself.  Using a 3:2:2 ratio of
    boric acid, TSP, and borax, and I can not get it all to go into
    solution.  The three parts amounts to about 48 grams of boric acid
    and the twos around 32 grams each, in a quart of water. 

    The mixture remains cloudy through boiling, and then allowing it to
    stand and cool the solution clears, but there is sediment on the
    bottom of the container.  Is this normal or am I doing something
    wrong?  I have used this clear solution while soldering and it seems
    to work OK. 

    I have tried different brands of borax and both powdered and
    granular boric acid, with the same results. The TSP is trisodium
    phosphate. I have also tried increasing the amount of water.  

Can anyone help? 
Thanks, Don


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project