>     Not a very good idea --you can expect very ragged flames with a
>     drilled out tip. 

    I never had any problem that way.  Some larger tips sometimes
    produce a flame that seems too high speed at times, which you can
    modify by running a small bud bur into the drill hole about 2/3ds the
    lenth of the bur head, with the size of the bur being only a little
    larger than the drill hole.  It flares the diameter of the exiting
    hole, and the gas stream slightly slows down.  Somewhat like the
    shape of a rocket motor nozzle.  The main visible effect is that the
    flame blows out less easily.  Do note that you need the gas and oxy
    pressures high enough so the flame is still decently brisk if you've
    done this to make a really large tip.  Too low a gas pressure and the
    flame can blow back into the torch body with the little torch, due to
    the small diameter of the gas line hoses, I think, Try, in doing this,
    not to have the exit diameter of the hole much larger than the
    internal bore of the tip tubing itself, for the same reason. 
    Fortunately, even drilling a little torch tip out to it's max, you're
    still not exactly talking about an excessively  large tip, at least
    not with natural gas or propane.  I'd not recommend this with
    acetylene or hydrogen at all. 

Peter

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project