    I've noticed several enquiries regarding engraving with a flex shaft
    so I wanted to reply with some information I hope will be useful. 

    I have found that engraving or carving with a flex shaft on metal to
    be very frustrating, though possible. Because of the usual low RPM
    associated with these motors there is a lot of "chatter", skipping
    and lines are not continuous. In carving wax though, my Foredom S is
    a very useful beast. 

    For detailing metal I found it necessary to finally take the plunge
    and buy a higher priced high speed hand piece. Mine is all metal,
    self lubricating and made by a dental supply company. It's highest
    RPM is 300,000 and though it does not hog out large amounts of metal
    like a flex shaft, it it's peerless when it comes to fine detail
    work. Because it has low torque. I am able to move smoothly (albeit,
    slowly) through hard material like metal. The only drawback to this
    tool is that it only accepts bits with a 1/16 mandrel. 

I hope this info is helpful.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project