    I built my own press I used 8x8 1/2 inch thick square beam with 1/2
    inch thick by 15 inch tall c channel in an H frame style the pins
    that hold up the table are 2/1/2  inch 4130 round bar the ram is
    made from a cat tractor hydraulic cylinder that I cut down  so it
    would have a 15 inch stroke the ram is 6 1/2inch in diameter and
    double acting so I can push and pull with it. I have never taken it
    to its max but in theory it should put out just under 200 tons
    approxamatley at 10,000 psi. I have never needed more than 20 tons
    honestly but I have a small tool complex if I can lift it by myself I
    dont want it if you need to hire a rigging company to move it [wow
    now your talken tools ]. There is a book put out by lindsy
    publications that tells you how to make deep drawing dies it is a
    reprint from books published around the turn of the century it is
    geared toward machinests and tool and die makers but it offers alot
    of real useful info and it is real inexpensive I think i paid like 7
    or 8 bucks for it and it is a couple hundred pages it also shows lots
    of diagrams as to how tins are made (altoid candy tins) and cans the
    same processes could easily be adapted to silver and other metals. 

Sincerely Kevin Potter


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project