Hi All,

    I have used HF acid for about six years in the lab. I consider
    myself lucky, since I haven't been burned. Last Friday, I cleaned a
    large quartz tube in 10% HF solution. We pour from a 49% wt. HF acid
    bottle, and never use full strength in any lab work. Most solutions
    are 2% HF concentration. 

    Proper handling procedures, personal protective equipment, safety
    showers, and a laboratory grade fume hood, all should be in place
    before using HF acid. 

    Most hospitals have little experience treating HF burns. When they
    are done injecting calcium into the exposed area, you will feel more
    like a pin cushion. 

    HF does not eat through the skin. Instead, it will absorb into your
    body very easily. It will take the calcium from your bone. 

    The best first aid treatment is water! At least 15 minutes of
    flowing water over the affected area is recommended by the MSDS for
    HF acid. Second, a 2% calcium gluconate gel treatment on the exposed
    area has been known to save some people from the calcium injections.
    Third, go to the hospital immediately! 

    All acids can be dangerous. I put HF acid on top of the list.
    Anywhere there is a toxic or highly reactive process, the fluorine
    ion shows up in the mix. 

Jeff

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project