| [Orchid] Dark Gray/Black Patina for Silver-plate | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: JHerman Date: Wed Jan 12 19:07:27 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Good morning folks, I've been using Technic's Tech-ox "P" for decades, but even diluted, it's very difficult to remove from items that have been plated. I don't like liver of sulfur for many reasons. Does ANYONE know of a good natural looking patina that really "sticks" to the metal? I need something that can easily be removed by hand with silver polish without having to scrub so hard that the plate itself come off. <edit> Related Pages: Patinas - Formulas http://www.ganoksin.com/borisat/nenam/patina-formulas.htm Surface Manipulation > Patination http://www.ganoksin.com/borisat/directory/library/subject/25/1 </edit> Many thanks, Jeffrey Herman, Silversmith Herman Silver Restoration & Conservation PO Box 72839 Providence, RI 02907 401/461-6840 Fax: 401/461-6841 E-mail: jeffherman AT silversmithing.com Web: http://www.silversmithing.com/silver ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project