From: RING14K Date: Tue Jan 11 20:18:30 2005 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Lee; When I make rings with a receiving area around the entire circumference, the best way is to make a flat band, then use two square pieces of wire, measure and hard solder so you have two bands that fit around the flat band. Then solder, drill holes and add prongs if not channel set. Don't over engineer your work, it just adds more ''work'.'' <edit - Message combined> OPPS LEE: I guess i didn't understand at first, The best way to approach your problem is to use pure silver on the inside band that you have done as i instructed. cut an inner bevel on one side of the sterling square band and make the square have a 5 thousands inset cut some vertical groves in the inner edge and hammer the square in with the flat band being hammered into the inset and grooves hammer flat file square and give it a dose of tec solder to hold it from spinning and fill any spaces. TEC solder will melt with little more than match heat just don't overheat!... Ringman ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project