>        I see you don't name ranaissance wax. I use it for protecting
>     copper patina and am very satisfied with it. The copper surface
>     looks very near the original patina. The only problem can be that I
>     don't us heat patinated copper for jewelry, only for panels, bowls
>     etc. So I am not sure about how skin-grease will effect the wax,
>     but it is worth a try. 

    I did a number of fold formed wall relief sculptures over 8 years
    ago. I colored the surfaces using  an oxy/acetelyne torch and then
    sprayed the surfaces with Krylon Crystal Clear acrylic coating. 8
    years later the colors are still intact, no discernable change.
    These pieces have been kept indoors except for one that I put
    outside last summer just to see if there would be any change. So
    far, there has been a slight deterioration. I am going to leave it
    outside all winter and then evaluate it. 

Joel Schwalb
joel4 AT optonline.net
www.schwalbstudio.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project