>     I am looking for the best lubricant to use in my 6" trim saw. 

    I would imagine that you would probably only use water for sawing
    gemstone material. That is what use here in Brasil - in copious
    quantities. 

>     Where can I get information on the correct R.P.M.for a faceting
>     machine for faceting semi precious and precious stones. 

    You should probably subscribe to one or more of the several
    facetting and lapidary discussion lists: 

    1) United States Faceters Guild. http://www.usfacetersguild.org/ To
    subscribe: usfgfaceterslist-subscribe AT yahoogroups.com a pretty
    technical discusion group. Many experts on this one 

    2) LAPIDARY ARTS and FACETERS DIGEST Published about once a week,
    except holidays from Spur,Texas POST TO EITHER LINK BELOW:
    lapidary AT caprock-spur.com faceters AT caprock-spur.com 

    3) "Ahlstedt's Professional Faceting" digest Despite it's name, it is
    more oriented to helping new facetters To interact with the list
    website - simply go to: http://groups.yahoo.com/group/PaulAhlstedt/
    To subscribe from this group, send an email to:
    PaulAhlstedt-subscribe AT yahoogroups.com 

Best regards,
Robert Lowe
Lowe Associates - Brasil
Gemstones, Rough, Specimens
Tucson - February 2 - 7, 2005 - GJX # 205
e-fax: 1-240-757-6022
e-mail: USA    < robertplowejr AT juno.com >
e-mail: Brasil < robertplowejr AT uol.com.br >

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project