From: Dave Date: Sat Dec 04 22:38:32 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Herb, > is there a simpler way to accomplish the scoring. I've not tried this technique on silver, but have used it successfully on aluminum. I see no reason why it wouldn't work on silver or any other precious metal for that matter. There's a tool available at hardware stores & others that sell sheets of plastic for windows etc. The tool is used to score the plastic prior to snapping it to the required size. The tool consists of a hard metal blade about .028" thick with a hook on the end & a plastic handle. If I remember, the tool was under $5 & it will last a long time. To score something, a metal straight edge is placed where the line is to be scored. The hook of the tool is then placed against the straight edge, pressed against the metal & pulled toward the edge. If a deeper groove is needed, additional scoring operations can be done. Dave ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project