    I too have tried to make copper grapes without success.  I have
    instead used glass beads with AB finish over black and produced
    acceptable looking tiny clusters.  However, and this is the reason
    for my post, I could not figure out how to make good clusters.  If I
    brazed wire first to make the cluster, I could not get the grapes
    attached without ruining the look. Using glass beads, I slipped them
    onto a brass head pin with a dab of super glue to keep the bead
    seated on the flat head. Then I twisted multiple wires to make the
    cluster and brazed the twisted wires to a base strand of copper wire
    about 1.5 to 2 inches from the beads.  But, more than 4 beads looked
    strange. I could not braze short stems for the clusters without
    breaking the glass beads or having the glue disintegrate.  Any
    suggestions would be much appreciated! 

    I have thought about painting real or fake grapes with PMC slip,
    firing (the grape will disappear leaving a shell) and then using some
    kind of patina to make it look real.  But how to attach into a
    cluster? 

Deb

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project