David & Greg:

    I truly appreciate your insights. The question became relevant for
    me as I have many customers who come from both sides of the fence.
    Some choose platinum for the inherent quality of patina over time
    lending to an antique look. I do have some that choose platinum for
    its durability and beauty in the newly finished state, but are
    disappointed at how quickly the polish finish is lost in daily wear.
    I have salespeople who actually steer customers towards 18kwg and
    away from platinum if they feel that the customer is going to fall
    in the latter category. We are simply looking for alternatives for
    the people who want and are willing to pay for the coveted metal,
    but who arent interested in the maintenance required to keep their
    high polished finish. 

    It is an age old conundrum, to be sure. I appreciate all opinions. 

Kimberlee A. Hughes
Donald Haack Diamonds
Charlotte, NC
www.donaldhaack.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project