From: Volpe, Constantino Date: Wed Nov 24 03:47:34 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Don't forget to look at your burnout process If you burn out too fast you can steam the wax in the flask and this can attach the investment causing breakdown Follow the instructions of the investment manufacturer based on the size flask you are using Tino Volpe Metallurgist, Technical Manager Tiffany & Co 300 Maple Ridge Drive Cumberland, RI 02864-8707 401-288-0124 Volpe AT Tiffany com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project