Jon...

    Need a bit  more information.  Are you  laying the silver over the
    stone or inlaying it into the stone?.  Is the silver heavy or thin? 
     Is it decorative or just flat and straight?  I suspect you would
    have problems getting the two to hold for very long.  If at
    all...the stone and silver surfaces at the meeting points would have
    to be roughed up a great deal to give the glue a purchase. 

    I would recommend you solder posts onto the back of the solder,
    drill holes in the stone and then glue the two together.  Otherwise,
    try grinding channels in the stone and inlaying the silver....if you
    cut the channels properly (undercut the lower portions) you can tap
    the silver in and it will hold mechanically. 

    Cheers from Don at The Charles Belle Studio in SOFL where simple
    elegance IS fine jewelry! dcdietz AT comcast.net

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project