========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Warren, I also add flux (I happen to like Battern's) to my joins after Pripping (?) and before adding the solder. I heat the Battern's till it relaxes and then add the solder. I normally use a small brush but then the metal is only warm from applying the Prip's. If I need to add more flux after the metal is hot, I use the tip of a pick. Your interest in using something like brass bristles sounds interesting. Suggest trying a small brass brush used in a Foredom....cut away all but a few bristles and see how that works. Cheers from Don at The Charles Belle Studio in SOFL where simple elegance IS fine jewelry! dcdietz AT comcast.net ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project