Hello Ann,

    lots of my customers ask me the same question: how do you clean
    Sterling Silver jewelry? 

    I always recommend toothpaste with whitening. Put a little bit in
    your palm, add some water and stir it into a paste, then use an old
    toothbrush and rub the paste onto the jewelry piece. When you are
    done, rinse it off, dry it and you will have a clean, well smelling
    piece which won't curse any irritation on sensitive skin which you'd
    get with Silver cloth or Silver dip, both of which are soaked with
    chemicals. It is a cheap and healthy way to clean all jewelry with
    or without stones. Hope that helps, 

Edith
Edith Schneider Jewelry
P.O.Box 52001
Palo Alto, CA 94303
es AT edithschneider.com
www.edithschneider.com
(650) 813 9755

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project